标准摘要
[中文适用范围]: 范围和对象 光伏 (PV) 模块是在其使用寿命期间持续暴露在室外的电气设备。高度腐蚀性的潮湿气氛@例如农业公司马厩的环境@最终可能会降低某些光伏组件的性能(金属部件腐蚀@某些非金属材料的性能恶化?C如保护涂层和塑料? C 通过氨同化)造成永久性损害,可能损害其功能和安全操作。该标准描述了可用于确定光伏组件对氨 (NH3) 的耐受性的测试序列。 IEC 61215、IEC 61646 和 IEC 61730-2 中完整描述了序列@中包含的所有测试(旁路二极管功能测试@除外)。本标准将它们结合起来,提供了评估光伏模块在溶解氨 (NH3) 浓度高的潮湿环境下运行时可能引起的故障的方法。本标准适用于平板光伏组件。该标准的结构严格遵循 IEC 61701。 [外文原描述]: IEC 62716:2013 describes test sequences useful to determine the resistance of PV modules to ammonia (NH3). All tests included in the sequences, except the bypass diode functionality test, are fully described in IEC 61215, IEC 61646 and IEC 61730-2. They are combined in this standard to provide means to evaluate possible faults caused in PV modules when operating under wet atmospheres having high concentration of dissolved ammonia (NH3). The contents of the corrigendum of May 2014 have been included in this copy.
英文名称Photovoltaic (PV) modules - Ammonia corrosion testing