标准摘要
[中文适用范围]: ISO 17190 的这一部分规定了测定聚丙烯酸酯 (PA) 超吸收性粉末中可吸入颗粒含量的方法。 注:商用聚丙烯酸酯高吸水性粉末由平均直径为 400 μm 至 800 μm 的颗粒组成,远大于可吸入颗粒的最大尺寸(约 10 μm)。 由于生产过程的原因,商业超吸收性粉末中可能存在极少量的可吸入颗粒。 [外文原描述]: This part of ISO 17190 specifies a method for determining the content of respirable particles in polyacrylate (PA) superabsorbent powders. NOTE Commercial polyacrylate superabsorbent powders consist of particles averaging 400 μm to 800 μm in diameter, which are much larger than the maximum size for respirable particles of approximately 10 μm. Due to the production process, very low amounts of respirable particles may be present in commercial superabsorbent powders.
英文名称Urine-absorbing aids for incontinence — Test methods for characterizing polymer-based absorbent materials — Part 11: Determination of content of respirable particles