标准摘要
[中文适用范围]: 规定了测定不饱和聚酯树脂反应性的方法,其特征是在80℃水浴中与催化剂一起加热时达到的最高温度以及混合物温度从65℃升至该最高温度所需的时间。 由于测试结果很大程度上取决于测试进行的条件,因此对这些条件进行了详细描述。 [外文原描述]: Specifies a method for the determination of the reactivity of unsaturated polyester resins as characterized by the maximum temperature reached when heated with catalyst in a water-bath at 80 °C and by the time taken for the temperatur of the mixture to rise from 65 °C to this maximum temperature. As the test results depend very much on the conditions under which the test is carried out, these conditions are described in detail.
英文名称Plastics — Unsaturated polyester resins — Determination of reactivity at 80 degrees C (conventional method)