镍合金 耐腐蚀和耐热 棒材和锻件 成分:58Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al 0.05Zr 0.006B 采用可消耗电极或真空感应熔炼 1975°F(1079°C)固溶处理

标准摘要

This specification covers a corrosion- and heat-resistant nickel alloy in the form of bars and forgings in the solutioned, stabilized, and precipitation heat-treated condition. Stock for forging shall be in the condition ordered.
英文名称Nickel Alloy, Corrosion- and Heat-Resistant, Bars and Forgings, 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B, Consumable Electrode or Vacuum Induction Melted, 1975 °F (1079 °C) Solution Heat Treated, Stabilized, and Precipitation Heat